Service Details
- Home
- Service Details
The preshipment inspections of tableware are very important to make sure all safety requirements, PO stipulations, production specifications are met. The quality checks will mostly follow below methods:
INSPECTION CHECKPOINTS | RESULTS | COMMENTS |
---|---|---|
A. Quantity check | NOT OK | |
B. Shipping marks & packing | OK | |
C. Labels, logos and colors | OK | |
D. Styles & measurements | N/A | |
E. Onsite safety and function tests | OK | |
F. Special requirements | OK | |
G. AQL workmanship (Visual inspections) |
NOT OK |
As the quality control inspections can happen at any stage of manufacturing, so there are:
The checklist for onsite quality inspection test will be like below:
INSPECTION CHECK LIST | COMMENTS | RESULT |
---|---|---|
Check if items stand properly when pieces are stacked up, if this test fail, please state the cause clearly on inspection report and take photos- 1)Stack the products (60 pieces for the plate/reference and 12 pieces for bowl/reference and cup/reference ); 2) Ensure they can stack properly and do not wobble or tilt over-S2 |
PASSED | |
Test the item for water leakage during the entire inspection period.-Fill the item with water then place onto a paper to check there is no leakage at all.-S2 | PASSED | |
Test the strength of the handle.--S2 | PASSED | |
Hand washing test -- --Wash the product with cotton fabric in cold water of room temperature (about 20--35degree) and hot water of tempertature (about 80 -- 90 degree) -- During washing, dip product into the water and wiping the whole surface of the product -No color should be removed from the item’s surface during the test and no printing, markings or paint should fade.-3 pcs | PASSED | |
Perform a fatigue test-On all adjustable parts. Do this 20 times.-S2 | PASSED | |
Test the fit of the lid. and lid can not falls off when the teapot is tilted toward 90 degrees-If the item has a lid - The lid should fit well.-S3 | PASSED | |
Perform a fitting test check-The lid should fit the base well.-II | PASSED | |
Compare the inspection sample with the approval sample.-II | PASSED | |
If the product is designed for use in a dishwasher and/or microwave oven, place it in a dishwasher and run the dishwasher for one cycle during the inspection period and also 10 minutes in the micro-wave oven.-If the product is designed for use in a dishwasher and/or microwave oven, place it in a dishwasher and run the dishwasher for one cycle during the inspection period and also 10 minutes in the micro-wave oven.-S2 |
FAILED | |
Check capacity (volume) by weighing the item or by using a capacity gauge ( the mug, bowl and the container claimed with the volumn)-The results must conform with the specifications.-S2 | PASSED | |
Perform a wobble test on a flat glass panel. Check both the top rim of the glass and the bottom.-There should be no wobbling of the base or the rim.-I | FAILED |
tableware quality assurance services, tableware 3rd party quality assurance, China tableware 3rd party quality assurance, tableware third party quality assurance services, tableware 3rd party quality assurance services in China, tableware 3rd party quality assurance services, China tableware 3rd party quality assurance services, China tableware quality assurance, China tableware third party quality assurance services, tableware third party quality assurance services in China, tableware quality assurance services in China, China tableware quality assurance services, China tableware third party quality assurance, tableware 3rd party quality assurance in China, tableware third party quality assurance, tableware third party quality assurance in China, tableware quality assurance in China
3rd party preshipment products goods factory onsite inline final Random AQL PSI TPI FRI DUPRO third party on-site in-line pre-shipment QA QC check control inspection services in China India Vietnam Thailand Malaysia Bangladesh Taiwan.