Service Details
- Home
- Service Details
The preshipment inspections of tableware are very important to make sure all safety requirements, PO stipulations, production specifications are met. The quality checks will mostly follow below methods:
INSPECTION CHECKPOINTS | RESULTS | COMMENTS |
---|---|---|
Measurements & sizes checks | N/A | |
Packaging, safety and drop tests onsite | OK | |
Aesthetic, visual defects, workmanship, surface and function inspections | NOT OK | |
Product specs, and special requirements checks | OK | |
On-site safety, regulation & function tests | OK | |
Quantity & assortment inspections | OK | |
Labels, markings, logos & barcodes checks | OK |
As the quality control inspections can happen at any stage of manufacturing, so there are:
The checklist for onsite quality inspection test will be like below:
INSPECTION LIST | COMMENTS | RESULT |
---|---|---|
Perform a wobble test on a flat glass panel. Check both the top rim of the glass and the bottom.-There should be no wobbling of the base or the rim.-I | N/A | |
Test the fit of the lid. and lid can not falls off when the teapot is tilted toward 90 degrees-If the item has a lid - The lid should fit well.-S3 | FAILED | |
Perform a fatigue test-On all adjustable parts. Do this 20 times.-S2 | PASSED | |
Test the item for water leakage during the entire inspection period.-Fill the item with water then place onto a paper to check there is no leakage at all.-S2 | PASSED | |
Check capacity (volume) by weighing the item or by using a capacity gauge ( the mug, bowl and the container claimed with the volumn)-The results must conform with the specifications.-S2 | PASSED | |
Check if items stand properly when pieces are stacked up, if this test fail, please state the cause clearly on inspection report and take photos- 1)Stack the products (60 pieces for the plate/reference and 12 pieces for bowl/reference and cup/reference ); 2) Ensure they can stack properly and do not wobble or tilt over-S2 |
PASSED | |
If the product is designed for use in a dishwasher and/or microwave oven, place it in a dishwasher and run the dishwasher for one cycle during the inspection period and also 10 minutes in the micro-wave oven.-If the product is designed for use in a dishwasher and/or microwave oven, place it in a dishwasher and run the dishwasher for one cycle during the inspection period and also 10 minutes in the micro-wave oven.-S2 |
PASSED | |
Hand washing test -- --Wash the product with cotton fabric in cold water of room temperature (about 20--35degree) and hot water of tempertature (about 80 -- 90 degree) -- During washing, dip product into the water and wiping the whole surface of the product -No color should be removed from the item’s surface during the test and no printing, markings or paint should fade.-3 pcs | FAILED | |
Compare the inspection sample with the approval sample.-II | PASSED | |
Test the strength of the handle.--S2 | FAILED | |
Perform a fitting test check-The lid should fit the base well.-II | PASSED |
tableware onsite inspection services, China tableware onsite inspection, China tableware onsite inspection services, China tableware 3rd party onsite inspection services, China tableware 3rd party onsite inspection, tableware third party onsite inspection, China tableware third party onsite inspection services, tableware 3rd party onsite inspection in China, tableware third party onsite inspection in China, tableware 3rd party onsite inspection services in China, tableware third party onsite inspection services, tableware onsite inspection services in China, tableware onsite inspection in China, tableware third party onsite inspection services in China, tableware 3rd party onsite inspection services, tableware 3rd party onsite inspection, China tableware third party onsite inspection